Reliability analysis of damaged concrete beams based on the rust crack width

BAI Yuliang,JIN Weiliang,YU Yifan,JIN Kangcheng (College of Civil Engineering and Architecture, Zhejiang University,Hangzhou 3lOo58,P.R.China)

Abstract: In order to investigate the degradation law of the durability of damaged concrete beams,by introducing the fatigue damage factor and the creep damage factor,the calculation model of the corrosion depth of the steel bar after corrosion cracking of the protective layer of the concrete beam with fatigue and creep damage was established.According to the durability design standard of concrete structure,the durability limit state equation controlld by the rust crack width was established.The Monte-Carlo numerical simulation method was used to calculate the reliability of six concrete test beams within the crack width limit.The sensitivity of the four parameters,including corrosion current density,concrete compressive strength,protective layer thickness and stee bar diameter,was calculated using the checkpoint method.The research results show thatthe reliability decreases from O.9 toO.1 with the increase of corrosion time and the increase of holding time for three months has little efect on the reliability of the beam after cyclic loading of 60% of the fatigue life times.

The increase of the protective layer thickness and the decrease of the diameterof the steel bar canboth improve thereliability of the beam and slow down the decline rate of the structural reliability at the early stage of corrosion of the steel bar. The steel bar diameter of 8mm can be used as a reference value for the durability design of damaged concrete beams. The sensitivity of the three parameters of corosion current density, protective layer thickness andsteel bar diameter is so relatively large that three parameters are the main influencing factors of durability limit state reliability.

Keywords: damaged concrete beams; rust crack width; limit state equation; reliability; sensitivity

在钢筋混凝土结构服役期间,环境中的有害介质侵入混凝土内部,导致钢筋表面的钝化膜破坏,引起钢筋的锈蚀。随着锈蚀量的增加,在钢筋与混凝土交界面出现锈胀裂缝,而钢筋锈蚀引起的混凝土结构开裂被认为是钢筋混凝土结构耐久性失效的主要原因[1。然而,对于实际工程结构,其往往遭受环境和荷载的耦合作用,加速了混凝土结构的开裂[2]。在环境和荷载作用的影响下,荷载裂缝的产生加速了钢筋锈蚀,而随着钢筋锈蚀程度的加深,混凝土表面锈胀裂缝宽度不断增大。当结构锈胀裂缝宽度达到限值时,严重影响结构的正常使用功能。

对于钢筋锈蚀引起的耐久性能退化问题,有学者们[3-15]围绕混凝土保护层锈胀开裂和锈胀裂缝等方面开展了大量研究,主要集中在钢筋锈蚀量和锈胀裂缝宽度方面。在钢筋锈蚀量方面,牛荻涛4通过电化学加速锈蚀试验,在试验数据的基础上进行回归分析,建立了混凝土保护层锈胀开裂时变形钢筋锈蚀深度计算模型;赵羽习等5建立了钢筋锈蚀导致的混凝土保护层锈胀开裂力学模型,并应用弹性力学分析得到了混凝土保护层锈胀开裂时的钢筋锈蚀率解析式;王胜年等通过对30多座海港实体工程进行调查和长达20a的长期暴露试验,给出了考虑影响因素较为全面的钢筋临界锈蚀深度计算公式;陆春华等假定钢筋均匀锈蚀,借助弹性力学和Faraday定律,建立了混凝土保护层锈胀开裂时刻的钢筋锈蚀率以及锈胀开裂时间计算公式;……

登录APP查看全文

猜你喜欢

耐久性宽度荷载
任意荷载下软土一维大应变非线性固结分析
基于数值模拟的切顶卸压后保护煤柱宽度研究
列车进站了!
基于相位切趾调制的非对称结构光栅滤波器设计与制备
竹集成材-竹胶板钉节点力学性能
桩板式路基湿接缝构造力学性能试验研究
锚杆抗滑桩组合边坡加固中抗滑桩参数研究
菱形挂篮悬浇施工关键结构施工受力分析
压力容器产品铭牌使用耐久性的思考
振动搅拌,基础设施耐久性的保障