双级固溶对高 Zn 含量Al-Zn-Mg-Cu合金组织及力学性能的影响
2025-08-09王卓王毅哲王家兴刘子涵周峻业刘英杨潇王立伟

Effect of dual stage solid solution on the microstructure and mechanical properties of Al-Zn-Mg-Cu alloy with high Zn content
WANG Zhuo1,²,WANG Yizhe1,²,WANG Jiaxing1,²,LIU Zihan 1,2 , ZHOU Junye ⋅1,2 LIU Ying1'²,YANG Xiao1,²,WANG Liwei1,2
(1.School of Materials Science and Engineering,Hebei University of Science and Technology, Shijiazhuang,Hebei O50o18,China; 2.Hebei Key Laboratory of Material Near-NetForming Technology,Shijiazhuang,Hebei O50ol8,China)
Abstract:Inordertosolve the problemofdificult dissolutionof second phaseparticlescaused byexcessve high Zncontent duringthe traditional heat treatment of Al- Zn-Mg-Cu alloy,the effects of different two-stage solid solution processes on the microstructure and mechanical properties of theas-quenchedand T6aged Al-Zn-Mg-Cualloy with high Zn content were investigated by using optical microscope(OM),scanning electron microscope(SEM),Vickers hardness tester and tensile testingunder room temperature.Theresultsshow that withthe increaseof the first-stage solid solution temperature,the strengthandhardnessof thealloyincrease,and theoverallmechanicalpropertiesofthematerialsimprove.Theelongationrate of thealloy increasesfirstlyandthendecreases withtheincreaseof thefirst-stagesolid solution temperature,andthetensile fractureshows toughnessfracture.Afterthealoysubjecting toatwo-step solution heat treatmentandquenching processat 460∘C for 1h and then at 475∘° for 2h ,thetensile strength,yield strength and elongation of the alloyare 580.5MPa , 465.3MPa and 13.6% ,respectively,indicating good comprehensive mechanical properties. The modulation of the temperature within the first stageof the two-stage solution treatment processisconducivetotheamelioration of the comprehensiveperformanceofaluminumaloymaterialswithahigh Zncontent.Itcanprovide theoreticalreference for improving the heat treatment process of aluminum alloy materials.
Keywords: the organization,structure, defects,and propertiesof materials;Al-Zn-Mg-Cu aloy;microstructure; solid solution;tensile property;fracture morphology
Al-Zn-Mg-Cu合金具有轻质高强、熔点低、流动性好、铸造性能佳和耐磨性高等特点,广泛应用于航空航天和高速列车等领域[1-2]。目前,现代航空和汽车工业的发展均对结构金属材料提出了高强度、轻量化的需求,同时也对铝合金材料的强度、硬度等性能提出了更严格的要求。提高综合性能的方法有2种:首先,提高 Al-Zn-Mg-Cu 合金中 Zn 元素所占的比例,可以使材料在时效过程中析出更多的 MgZn2 相,最终提高产品的机械性能3;其次, Al-Zn-Mg-Cu 合金属于可热处理强化的超高强铝合金,已知 Al-Zn-Mg-Cu 合金中的强化效应主要来源于时效过程中形成的析出相,析出相的几何特征(尺寸、形貌及分布等)决定了铝合金最终的综合性能[4]。固溶处理是指将合金加热至高温单相区恒温保持,使过剩相充分溶解到固溶体中,然后快速冷却得到过饱和固溶体[5]。这一方法的实施对于后续时效处理过程中析出相的析出能力具有显著影响,进而直接关系到合金在时效强化后的性能表现[6]。目前对于固溶处理的研究,大多着眼于双级固溶处理。与传统的单级固溶效果相比,双级固溶在突破单级固溶温度上限的同时使材料的再结晶程度更小,第二相回溶更充分,可以在更低的热输入下取得更优异的性能]。
目前,针对常规 Al-Zn-Mg-Cu 高强铝合金的双级固溶处理研究较为集中[8],然而,对于 Zn 含量大于 7% (质量分数,下同)的超高强铝合金而言,其更高的合金化程度使单级固溶处理更为困难,难以获得符合要求的性能。因……