APP下载

不同改性处理对橡胶木抗菌性能影响研究

2025-08-03张倩吕蕾周亚菲尚欣宇

森林工程 2025年4期
关键词:黑曲霉二氧化钛改性剂

中图分类号:S794.1 文献标识码:A DOI: 10.7525/j.issn.1006-8023.2025.04.014

Abstract:Usingrubberwoodasrawmaterial,orthogonal experimentaldesign wasused to exploretheinfluenceof silverloaded nano itanium dioxide impregnated heat treatmentonthe mold and corrosionresistance of rubberwood,and compared themold and corrosion resistance,dryshrinkage and wet swelling properties ofthe control timber,heat-treated timber,silver-loadednano titanium dioxide impregnatedtimberandsilver-loaded nano titaniumdioxideimpregnated heat-treated timber,andtheinfluence mechanismof diferent modification treatments onthe physicochemical properties of the timber wasrevealedthrough the means of electron microscopy,XRD(X-ray difraction).Theresults showed that the optimal process of silver-loaded nano titanium dioxide impregnated heat treatment was 16O C,2.5 h,1. 5% silver loading,1.5mg/mL modifierconcentration,6O min vacuum impregnation time,atthis time,the modified timber had thegreatest efficacy inthe preventionofAspergillusnigerandPenicilliumcitrinum,both of them were 100% ,and the modified timberhadthe smallestrateofqualitylossunderthe influenceof white-rotfungus and brown-rotfungus,which were 2.36% and1.9 % ,respectively. Compared with the control timber,heat-treated timber and silver-loaded nano titaniumdioxide impregnated timber,silver-loaded nano titanium dioxide impregnated heat-treated timber hadthelowest wetswellng anddryshrinkage,theradial,tangentialand volumetric water-absorbing wetswellingrate was reduced by 31. 34% -36. 36% compared with that of the control timber,the radial,tangential and volumetric moisture-absorbing wet swelling rate was reduced by 41. 06% -61. 7% compared with that of the control timber,the radial, tangential and volumetric air-drying dry shrinkage rate was reduced by up to 23.28%-32. 24% compared with that of the control timber.

Thesilver-loadednanotitaniumdioxideimpregnatedheat treatmentcanrealizetheuniformloadingofsilver-loaded nano titanium dioxideparticles in wood,which cancomprehensively improvethe moldand corrosionresistance and dimensional stability of wood,and realize the excellent wood modification effect.

Keywords:Silver-loaded nano titanium dioxide;heat treatment;mold and corrosion resistance;wet swelling proper ties;wood modification

0 引言

橡胶木(Heveabrasiliensis)作为一种重要的热带木材,因其生长迅速、纹理美观和易于加工等特性而被广泛应用于家具、建筑和装饰等领域1。然而,橡胶木也存在一些固有的问题,如易腐、易霉变和尺寸稳定性差等,这些问题限制了其更广泛的应用和长期的使用寿命[2-3]。因此,对橡胶木进行改性处理,提高其耐久性和稳定性,成为当前研究的热点。

国内外关于橡胶木改性技术的研究已经取得了显著的进展。热处理作为一种传统的改性方法,通过高温处理木材细胞壁物质(主要是半纤维素和木质素)发生热解及分子结构重组,导致吸湿性羟基数量减少,结晶区的比例增加,从而可以改善木材的耐久性和尺寸稳定性,但可能导致木材力学性能的下降[4-6]。王秉泉等[7]探究了双酸酐-植物油热联合处理工艺对条纹乌木进行改性处理,结果发现在 90°C 油热处理温度下,马来酸酐预处理2h,衣康酸酐预处理4h,在抗湿和抗膨胀性上均比未经酸酐处理的样品显著改善,在油热工艺前设置预处理,可以改善木材在热处理过程中机械性能的下降。有学者探究了高温热处理对白蜡木、柞木和杉木等木材的性能影响,研究发现,在温度低于180∘C 时,木材硬度、抗弯强度和弹性模量等指标呈现增加趋势;当温度超过 180∘C 时,木材的力学性能呈现明显下降的趋势[8-9]。不同热处理工艺参数、树种等对木材力学性能的影响规律存在差异,低温短时间的热处理对其力学强度的影响不大,高温且长时间的处理会造成其力学强度的降低。……

登录APP查看全文

猜你喜欢

黑曲霉二氧化钛改性剂
APAO/EVA复合改性沥青的常规和流变性能研究
二氧化硅包裹锐钛矿型二氧化钛处理木材的老化性能研究
聚乙二醇处理对杞柳软化效果的影响
复合微生物菌剂发酵芭蕉芋试验研究
石墨烯-二氧化钛复合粉体改性皮革涂饰剂的应用研究
一种纸质档案装订用水性胶粘新材料制备及性能研究
常见菌体发酵过程中的生物学原理
六景至钦州港公路改性沥青路面设计与性能评价