APP下载

1780热轧厂热卷箱卷型控制技术

2018-08-03金永江

中国科技博览 2018年28期

[摘 要]热卷箱在1780热轧厂的使用,确保生产薄规格的不锈钢及碳钢时精轧轧制稳定性。但在使用过程中也遇到了卷偏的现象。即在热卷箱在正常卷取过程中当卷到尾部七至八圈开始,钢卷容易出现松卷并出现类似成品钢卷卷取过程的塔形的现象,极易造成钢卷在开卷过程中头部跑偏而卡住2#工位侧导板而废钢。通过调整热卷箱弯曲辊辊缝打开延迟、粗轧RDT温度、中间坯厚度、弯曲辊和1#工位超前率以及弯曲辊辊缝打开速度,成功解决了热卷箱卷偏的问题,确保了热轧轧制过程稳定。

[关键词]热卷箱;弯曲辊;轧制稳定性;卷偏

中图分类号:TG506 文献标识码:A 文章编号:1009-914X(2018)28-0021-02

[Abstract]Coil box is used in 1780 hot strip rolling plant, ensure the production of thin gauge rolling stability of stainless steel and carbon steel finishing. But it was encountered in the course of using the volume. Hot coil box in the normal course of winding when the volume to the end starting seven or eight laps, steel coils were proned to pine volume and similar products during the coil winding Tower. Coil might be easily caused during the process of unwinding the head misalignment, and Stuck in the 2# coil-roller side guides and steel scrap. By adjusting the coil box bending roll seam opening delay, roughing RDT temperature, intermediate billet thickness, bending roller and a # stations ahead of rates and bending roll seam opening speed,we successfully resolved the partial volume coil box problems and ensure the stability of hot rolling process.

[Key words]Coil box, Bending rolls, Rolling stability, Roll bias

1 前言

宝钢不锈钢有限公司热轧厂设置有带侧向保温隔热屏的无芯轴钢卷转移式热卷箱,安装于粗轧机的延伸辊道和精轧切头飞剪之间,将粗轧机轧制成的带坯卷成热钢卷,然后通过其中的开卷机构将热钢卷的头部(卷取前的尾部),引入夹送辊进行压平矫直,并使带钢的头部能顺利地通过切头飞剪和精轧前除鳞箱后送入到精轧机。

该热卷箱可减少中间坯头尾温差、降低精轧机组能耗、改善产品表面质量。有利于提高薄规格的不锈钢及碳钢生产时精轧轧制稳定性。但在使用过程中也遇到了卷偏的现象。

卷偏,即是在热卷箱在正常卷取过程中当卷到尾部七至八圈开始,钢卷容易出现松卷并出现类似成品钢卷卷取过程的塔形的现象。该现象一旦出现,在接下来的开卷过程中带头极易发生跑偏并卡住2#工位侧导板,使得开卷无法继续进行而废钢。……