【摘要】混凝土中适量的掺入普通减水剂,就可以在保证混凝土工作性、强度和耐久性等的前提下,尽可能地减少拌合用水量,降低水灰比,这就是普通减水剂的减水作用。本文讨论了普通减水剂对新拌混凝土减水率的影响。
【关键词】减水剂;新拌混凝土;减水率;影响
Effect of ordinary water - reducing agent on water reduction of fresh concrete
Lu Zhong-fu
(Zhongfu Construction Group Co., LtdShaoxingZhejiang312000)
【Abstract】The amount of concrete mixed with ordinary water-reducing agent, you can ensure the workability of concrete, strength and durability under the premise of as much as possible to reduce the amount of mixed water, reduce the water-cement ratio, which is the ordinary water-reducing agent effect. This paper discusses the effect of ordinary water reducing agent on the water reduction of fresh concrete.
【Key words】Water - reducing agent;Fresh concrete;Water reduction rate
1. 前言
1.1减水率是坍落度基本相同时,基准混凝土与掺外加剂混凝土单位用水量之差与基准混凝土单位用水量之比。
1.2拌合用水量的大小直接关系到混凝土的强度和耐久性。根据水泥水化硬化理论,水泥全部水化的理论水灰比约为0.227,但在配制混凝土时为了保证足够的流动性,水灰比常常大于此值。这些水化过程不需要的水分称为游离水。
1.3游离水可能停留在混凝土结构的毛细孔中,也可能蒸发形成混凝土中的空隙,造成混凝土强度降低,耐久性变差。
1.4混凝土中适量的掺人普通减水剂,就可以在保证混凝土工作性、强度和耐久性等的前提下,尽可能地减少拌合用水量,降低水灰比,这就是普通减水剂的减水作用。而拌合用水量的大小直接关系到混凝土的强度和耐久性。普通减水剂的实际减水率与许多因素有关,主要有以下两类:(1)普通减水剂的类型、掺量及掺人入方式;(2)混凝土的设计工作性和水灰比、水泥标号、骨料类型、集灰比(骨料/水泥比)、粉煤灰等掺合料的种类及用量等。
2. 它们的影响具体如下。
2.1普通减水剂类型。
表1是工作性和普通减水剂掺量一定时,不同类型普通减水剂的减水率。……