对水工混凝土渗漏处理与预防措施的探讨

2012-06-04黄万佳

城市建设理论研究 2012年13期

黄万佳

摘要:水工混凝土建筑物的各种病害和缺陷往往始发与建筑结构的外表面,如裂缝、渗漏等,渗漏是水工混凝土建筑物的常见的一种老化病害现象。本文探讨了有效的防护措施及堵漏防水施工等施工方法,指出水工混凝土堵漏防水是一项系统工程,并针对渗漏产生的原因进行了分析,并提出了相应的处理措施。

关键词:水利工程,渗水,堵漏防水施工,防水措施

Abstract: the hydraulic concrete structures of disease and often initial and building structure defects of the outside surface, such as crack, such as leakage, leakage is the concrete buildings of hydraulic a common phenomenon of aging. This paper probes into the effective protective measures and its waterproof construction, construction method, and points out that the hydraulic concrete plugging waterproof is a system engineering, and in the light of the causes of the leakage are analyzed, and the corresponding treatment measures.

Keywords: water conservancy project, seepage, plugging waterproof construction, waterproof measures

中图分类号:TV 文献标识码:A文章编号:

1、渗漏形成及原因

渗漏是常见的水工混凝土缺陷。渗漏给水工建筑物带来一系列的不利影响,危及建筑物的安全运行,会使建筑物产生溶出性侵蚀,即外渗将水泥中的CaO溶化析出,变成氢氧化钙,在出水口处形成碳酸钙结晶等溶蚀状态,从而使混凝土强度下降。

导致渗漏的主要原因:一是结构体中有裂缝和架空,形成渗水通道;二是结构体的止水设施质量差或浇空、浇翻、漏埋,使止水失去效果。如果库水具有较强的化学侵蚀性,也会在长期的化学侵蚀下,使坝体形成渗漏。因为渗漏和溶蚀的共同作用,将加速坝体渗漏破坏。尤其是当库水中含有硫酸盐时,与混凝土中的Ca(OH)2反应生成CaSO4,会产生体积膨胀,而CaSO4与混凝土中的C3A反应生成硫铝酸钙,会产生第二次体积膨胀,膨胀应力使混凝土胀裂变酥,极大降低混凝土强度,使混凝土遭到破坏,甚至成粉末状。

2、渗漏发生的部位及表征

1) 大面积渗水。一般大面积渗水一般发生在基础底板,主要原因是基面四周基坑降水应在垫层以下,施工中达不到应有水平,造成排水不良,如遇雨天停电或出现其他机械故障,基坑水位上涨,淹没垫层,不具备灌注混凝土条件,为抢进度,带水施工。……