以异佛尔酮二异氰酸酯(IPDI)和巴斯夫扩链剂-4370(ADR-4370)为扩链剂,采用熔融挤出法制备扩链改性聚(3-羟基丁酸酯-co-4-羟基丁酸酯)[P(3HB-co-4HB)].使用毛细管流变仪、哈克转矩流变仪、力学性能测试仪及扫描电子显微镜等研究扩链剂种类及添加量对P(3HB-co-4HB)流变性能、熔体加工稳定性、力学性能及断面形态的影响.结果表明:两种扩链剂单独或配合使用均能显著提高熔体表观黏度,改善加工性能、断面形态及力学性能.IPDI的添加量为1%时,体系综合性能最佳,其拉伸强度、断裂伸长率和缺口冲击强度分别比纯P(3HB-co-4HB)增加了22%、234%和95%.
聚(3-羟基丁酸酯-co-4-羟基丁酸酯);熔融扩链;流变性能;力学性能;断面形态
Abstract:IPDI or ADR-4370 was selected as chain extender to prepare modified poly(3-hydroxylbutyrate-co-4-hydroxylbutyrate) via melting extrusion. Capillary rheometer,HAKKE torque rheometer and scanning electron m icroscope(SEM) were used to characterize the effects of various chain extender and their dosage on the rheological properties,melt processing stability,mechanical properties and fracture morphologies of P(3HB-co-4HB). The results show that both single or match use of two chain extenders can significantly increase the melt apparent viscosity and improve the processing properties,fracture morphologies and mechanical properties of P(3HB-co-4HB). The comprehensive properties of P(3HB-co-4HB)achieve the optimum w ith IPDI at 1%. Compared w ith pure P(3HB-co-4HB),the tensile strength,break elongation and notched impact strength are higher 22%,234% and 95%.
Keywords:poly(3-hydroxybutyrate-co-4-hydroxybutyrate);melt chain-extension;rheological properties;mechanical properties;fracture morphology
聚羟基丁酸酯(PHB)是一类可热塑加工成型和完全降解的聚酯塑料[1–4],符合环境保护与可持续发展战略的要求,因此在医学、药物、工业、农业等领域具有其独特的应用.但其生产成本高、热稳定性较差、脆性大、熔体强度较低等不足[5]限制了其应用范围.与PHB相比,聚(3–羟基丁酸酯-co-4-羟基丁酸酯)即P(3HB-co-4HB)的热稳定性和韧性得到了很大程度的改善,但其加工性、流变性及力学性能并不能完全满足使用的要求.本文分别选取异佛尔酮二异氰酸酯(IPDI)和巴斯夫扩链剂-4370(ADR-4370)为扩链剂,通过熔融挤出方法,对P(3HB-co-4HB)进行扩链改性,旨在通过……