4H-SiC同质外延材料堆垛层错缺陷的表征与研究
2025-08-03芦伟立房玉龙李帅王启蘅韩明睿王波





Characterization and Research on Stacking Faults and Defects of 4H-SiC Homogeneous Epitaxial Wafer
LU Weili FANG Yulong\"LI ShuaiWANG QihengHAN MingruiWANG Bc (The 13th Research Institute of China Electronics Technology Group Corporation)
Abstract: The stacking faults and defects of SiCepitaxial materials grown bya horizontal single wafer epitaxial CVD reactorwasstudied.Thethickness anddefectsofSiCepitaxial materialswerecharacterized,tested,andstatistically analyzedusing theFourier transform infrared spectrometer and surface defect analyzer.The generation mechanism and extensionmodelofstacking faultsofSiChomogeneous epitaxialmaterials werestudied,andtheinfluenceofSiCsubstrate TSD and BPD dislocation density on the stacking faults density was researched.Through optimization of epitaxial temperatureand improvementof bufer layer process,thedensityofstacking faults inepitaxial materials was reduced to less than 0.1/cm2 . High-quality SiC epitaxial materials can further meet the needs of various SiC power electronic devices.
Keywords:SiC;epitaxy; defects; stacking faults
碳化硅(SiC)作为宽禁带半导体材料的代表,相较于传统硅材料,具有高10倍的击穿电场强度、高2倍的电子饱和速度、高3倍的禁带宽度和高3倍的热导率,尤其适用与制作高频、高压、大功率的SiC电力电子器件[-3]。SiC电力电子器件可以广泛应用于新能源汽车、光伏逆变、数据电源、风力发电、机车牵引和柔性电网等领域[4-5]。尤其近几年新能源汽车领域和光伏产业迅速发展,助推SiC全产业链技术水平和产业规模迅猛发展。
SiC外延材料缺陷种类繁多,其中一类是外延过程中工艺不稳定造成的缺陷如:三角形缺陷、胡萝卜缺陷、掉落物缺陷、凹坑缺陷等,另外一类是衬底中位错、机械损伤等延伸或导致外延过程中成核产生的位错或缺陷,如:划痕、基平面位错,螺旋刃位错、堆垛层错(StackingFaults,SF)等。在过去几年中,SiC外延技术及外延材料生产能力迅速提升,尤其以外延材料三角形缺陷、胡萝卜缺陷、掉落物等致命缺陷的控制技术迅速发展]。为进一步提高器件成品率,外延材料的其他缺陷仍需进一步降低,其中外延过程中产生的SFs会造成器件反向漏电增大以及降低击穿电压,同时在大的电流应力下会产生延伸扩展,引起正向电压漂移等问题,严重影响了SiC器件的性能,逐渐成为SiC材料和器件的关注热点之—[7-8]。SiC外延材料中SFs种类很多,其成核原因也众说纷纭,已报道的产生原因主要包括衬底中SF、贯穿性螺位错(ThreadingScrewDislocation,TSD)和基平面位错(BasalPlaneDislocation,BPD)等位错的转化。2009年HASSAN等人研究发现衬底中的堆垛层错会扩展至外延层中,形成梯形形貌的Bar-shape(20 SF[9] 。……