Ni-Sn-Ni焊点界面金属间化合物的微观形貌演变研究
2023-06-07赵志豪李五岳李国俊田野
赵志豪 李五岳 李国俊 田野



摘 要:【目的】研究Ni-Sn-Ni微焊点在固液反应条件下界面金属间化合物(Intermetallic Compounds,IMCs)的生长及形貌变化。【方法】采用精密夹具调控的Ni-Sn(20 μm)-Ni作为样品,通过SEM观察等温条件下Ni-Sn-Ni不同时间点横截面的微观组织结构,并通过EDX对界面处生成的IMCs进行分析。【结果】在Ni-Sn反应的界面处仅生成一种单相IMCs,为Ni3Sn4,该界面IMCs的生长速度由快变慢最后趋于平缓。此外,界面IMCs的形貌随时间由针状转变为棒状后再转变为块状。【结论】在Ni-Sn固液反应中,界面IMCs的生长速度及形貌随键合时间的增加发生显著变化。
关键词:Ni-Sn-Ni微焊点;界面反应;金属间化合物
中图分类号:TG454 文献标志码:A 文章编号:1003-5168(2023)10-0088-04
DOI:10.19968/j.cnki.hnkj.1003-5168.2023.010.018
Abstract: [Purposes] In this paper, the growth and morphology changes of interfacial intermetallic compounds (IMCs) in Ni-Sn-Ni micro-solder joints under solid-liquid reaction conditions were studied. [Methods] In this experiment, Ni-Sn (20 μm)-Ni regulated by precision fixtures were used as the sample, the microstructure of the cross-section of Ni-Sn-Ni at different time points under isothermal conditions was observed by SEM, and the IMCs generated at the interface were analyzed by EDX. [Findings] Only a single-phase IMCs Ni3Sn4 was formed at the interface of Ni-Sn reaction, and the growthrate of IMCs at the interface changed from fast to slow and finally flattened. In addition, the morphology of interfacial IMCs changes from needle-like to rod-like and then to bulk-like with time. [Conclusions] During the Ni-Sn solid-liquid reaction, the growth rate and morphology of interfacial IMCs changed significantly with the increase in bonding time.
Keywords: Ni-Sn-Ni micro-solder joints; interface reaction; intermetallic compound
0 引言
物聯网、大数据及5G等技术的快速发展要求芯片性能更高、尺寸更小、可靠性更好。而二维封装已经不能满足芯片未来发展的需求[1]。基于硅通孔技术的三维封装技术因具有高集成度、低功耗和高运行速率,将成为未来发展的主流方向[2-3]。
在三维封装中,随着芯片不断向多功能化、微小化的方向发展,导致微焊点的尺寸不断减小。而微焊点尺寸的减小将直接导致微焊点中金属间化合物(Intermetallic Compounds,IMCs)的比例显著增加,进而使IMCs的性能成为影响微焊点性能的决定性因素之一。影响IMCs性能的因素主要有IMCs的材料、IMCs的生长等[4]。Ni通常作为焊盘中的扩散阻挡层,所以在Sn钎料微焊点中常出现Ni-Sn-Ni微互连结构[5]。因此,研究Ni-Sn-Ni焊点界面IMCs的微观形貌演变具有重要意义。
目前Wang等[6]研究了在280 ℃的键合温度下Ni-Sn-Ni焊点在不同互连高度下的微观形貌,发现其微观形貌主要由针状及块状两种IMCs。……