核级316NG控氮奥氏体不锈钢的局部腐蚀行为

2017-10-14,,

腐蚀与防护 2017年10期
关键词:不锈钢

, ,

(中国核动力研究设计院 核燃料及材料国家重点试验室,成都 610041)

核级316NG控氮奥氏体不锈钢的局部腐蚀行为

刘思维,罗强,王理

(中国核动力研究设计院核燃料及材料国家重点试验室,成都610041)

采用电化学测试法、点腐蚀试验法、盐雾腐蚀试验法和慢应变速率测试法,分别对比研究了核级316NG控氮奥氏体不锈钢和321奥氏体不锈钢的局部腐蚀行为,并利用扫描电子显微镜、光学显微镜等分别观察腐蚀后不锈钢的表面形貌。结果表明:316NG和321不锈钢晶间腐蚀再活化率分别为3.83%和4.47%,点腐蚀速率分别为10.74 g/(m2·h)和45.97 g/(m2·h),盐雾腐蚀速率分别为2.14×10-2g/(m2·h)和12.32×10-2g/(m2·h),应力腐蚀开裂敏感指数分别为0.078和0.10;316NG不锈钢中N和Mo元素提高了其耐局部腐蚀性能,因此其耐局部腐蚀性能均优于核电站结构材料321不锈钢的。

控氮奥氏体不锈钢;316NG不锈钢;321不锈钢;局部腐蚀

Abstract: The localized corrosion behavior of nuclear grade nitrogen-containing austenitic stainless steel 316NG was studied in comparison with austenitic stainless steel 321 by electrochemical method, pitting corrosion testing, salt spray testing and slow strain rate testing (SSRT), respectively. The surface morphology of the stainless steel after corrosion was observed by optical microscopy and electron scanning microscopy. The results show that for stainless steels 316NG and 321, the rates of reactivation were 3.83% and 4.47%, the pitting corrosion rates were 10.74 g/(m2·h) and 45.97 g/(m2·h), salt spray corrosion rates were 2.14×10-2g/(m2·h) and 12.32×10-2g/(m2·h), and the sensitivity indexes of SCC were 0.078 and 0.10. The localized corrosion resistance of stainless steel 316NG was better than that of stainless steel 321 because of the existence of Mo and N in the stainless steel 316NG making localized corrosion resistance improve.

Keywords: nitrogen-containing austenitic stainless steel; stainless steel 316NG; stainless steel 321; localized corrosion

奥氏体不锈钢由于具有优良的力学性能、耐腐蚀性能,因此被广泛作为核电站主管道和堆内构件材料。目前,核电站多建于沿海地区,常年处于海洋大气中,且在高温、高压下运行,服役环境恶劣,因此核电站广泛使用的奥氏体不锈钢结构材料存在应力腐蚀和点腐蚀等局部腐蚀现象[1-3]。316NG不锈钢为我国研发的新型核级控氮奥氏体不锈钢,由于其采用了N作为强化元素,并通过二次精炼技术实现了材料的低碳化,从而克服了曾大量应用的稳定化奥氏体不锈钢因碳含量高给其带来的不利影响,提高了材料的耐局部腐蚀性能[3-5]。

本工作以国产新型……

登录APP查看全文

猜你喜欢

不锈钢
超级英雄不锈钢侠
中低碳系列马氏体不锈钢开发与生产
孤胆不锈钢侠——米格-25
80t不锈钢GOR底吹转炉工艺设备改造
TP347不锈钢蛇形管制造工艺
不锈钢扎啤桶维修经验
不锈钢微钻削的切屑形成与仿真分析
FV520(B)不锈钢焊接接头的断裂性能
关于不锈钢厚壁管的焊接
1Crl2Ni3MoVN不锈钢TIG焊接工艺及接头性能