摘要:通过对不同竹炭含量的PA66/竹炭混合改性材料的紫外-可见光Abs吸光度、DSC/TG热分析实验及傅里叶红外吸收光谱分析发现:加入微米级的竹炭微粉可使PA66/竹炭混合材料对紫外线的防护能级明显增强,竹炭含量为1%~5%时即可达到完全防护;混合改性材料的热稳定性降低;根据在波数1 125 cm`(-1)处吸收峰的强度大小,可定性地鉴别混合物中加入竹碳粉的量。
关键词:竹炭微粉;PA66;Abs吸光度;DSC/TG热分析
中图分类号:TS151
文献标志码:A
DOI:10.3969/j.issn.1671-6906.2015.03.008
Abstract:Based on the study of the key performance of micron charcoal powder, through the different levels of charcoal in PA66 / charcoal mixed modified materials' UV - visible absorbance Abs, DSC / TG thermal analysis experiments and fourier transform infrared absorption spectroscopy, it is found that adding micron charcoal powder can enhance UV protection level of PA66 / charcoal powder mixed materials significantly, and full protection level can be achieved when its content is 1% to 5% of charcoal; mixed modified thermal stability is decreased. According to the wave number 1125 cm`(-1) absorption peak,it can qualitative identify the quality of carbon powder, the methods and results can provide a reference for similar studies.
收稿日期:2014-08-09
基金项目:纺织服装产业河南省协同创新中心项目资助
作者简介:王怀芳(1980-),女,山东临沭人,副教授,博士。
文章编号:1671-6906(2015)03-0041-03
竹炭微粉具有优良的导电、导热、吸收屏蔽紫外线及净化空气等功能,将其以一定比例与其他纤维材料共混改性可得到新的功能性纤维[1-2]。本研究以PA66聚酰胺为基本材料,通过在PA66-甲酸混溶体中均匀混入不同比例的竹炭微粉并制备成PA66/竹炭膜,研究了竹炭微粉的添加量对PA66的紫外线屏蔽防护功能及热稳定性的影响。
1实验
1.1实验材料及主要仪器
(1)实验材料为竹炭微粉(上海海诺炭业有限公司)、PA66[-NH(CH2)6-NHCO(CH2)4CO]n切片(平顶山神马集团帘子布厂) 、白包带黄色颗粒(密度1.10~1.14 g/cm3、马丁耐热50~60 ℃、相对粘度2.45、体积电阻率1.83×1015Ω cm、熔点252 ℃、熔化温度260~290 ℃、热分解温度≥350 ℃,具有优良的耐磨自润滑机械强度)、甲酸HCOOH(80%,天津盛兴化学试剂有限公司)。
(2)主要仪器设备为LS-POP9激……