非易失闪存中堆叠电容的精度控制研究与改善
2020-08-31郎玉红陆振杰祁鹏
郎玉红 陆振杰 祁鹏



摘 要: 讨论了非易失闪存(NOR Flash)器件中ONO介质层厚度的精度控制.通过归一化不同密度器件分组,优化多层复杂薄膜的光学量测精度,优化氮化硅层的均匀性,实现了对ONO介质层厚度更精确的控制.结合光学厚度与电性厚度的相关性,可以及时得到ONO工艺的安全窗口.
关键词: 闪存; 堆叠电容; ONO介质层; 读写速度; 数据存储能力
中图分类号: TN 47 文献标志码: A 文章编号: 1000-5137(2020)04-0478-05
Abstract: The precision control of the thickness of the ONO structure in NOR Flash device was discussed in the paper.The control of the thickness of the ONO structure became more precisely by means of normalizing the different density groups of devices,optimizing the optical measurement accuracy of multilayer complex films as well as the uniformity of silicon nitride layer.The safe ONO process window could be obtained in time by combining the relationship between the optical thickness and electrical thickness.
Key words: flash; stacked capacitance; ONO structure; I/O speed; data storage capacity
0 引 言
闪存主要分为NAND和非易失闪存(NOR Flash),NOR Flash存储器具备随机存储、可靠性强、读取速度快、可执行代码等优点.很多终端电子产品因内部指令执行、系统数据交换等功能,需要配置相应容量的代码存储器,这使低容量的NOR Flash存储器在应用中具备性能和成本上的优势,得到了广泛的应用,成为不可或缺的重要电子元器件.随着5G基站建设、汽车智能化的不断推进,真正无线立体声(TWS)耳机功能的日益增多,NOR Flash有望迎来更多需求[1].根据数据显示,中国NOR Flash新增市場规模从2015年的3.54亿元增长至2018年18.94亿元,预计到2022年,中国NOR Flash新增市场规模合计达到55.85亿元[2].
作为一种非挥发性存储器,NOR Flash具有高器件密度、低功耗和可电重写性等特点,被广泛应用于便携式电子产品中[3].NOR Flash与场效应晶体管(FET)[4-5]的差别在于栅极由控制栅、浮栅和ONO层构成.ONO介质层的构成为:上层氧化层(O)、中层氮化物(N)、下层氧化层(O).NOR Flash主流的ONO结构主要由炉管沉积完成.采用炉管低压化学气相沉积(LPCVD)工艺进行ONO介质层的制备,由3道炉管单独完成,分为:1) 底层氧化层的制备;2) 中……