APP下载

铬掺杂对硅酸铁锂电学性能影响的计算机仿真研究

2020-05-06王圣智蒋闯房勇

王圣智 蒋闯 房勇

【摘  要】硅酸铁锂是一种锂离子电子的正极材料,由于其晶胞在理论上可允许可逆脱嵌两个锂原子,使得其理论比容量有巨大的提升空间,加上原料易得、无污染及成本低的优势,受到了人们的重视。正极材料掺杂被认为是改善其导电性能的有效途径。论文通过运用基于第一性原理方法的计算机仿真技术,对铬掺杂硅酸铁锂的结构和导电性能的影响进行了计算机仿真研究,结果表明未掺杂的硅酸铁锂其带隙快读为2.44eV,掺杂铬之后硅酸铁锂带隙减小为2.31eV,表明铬掺杂可提高硅酸铁锂的导电性能。

【Abstract】Li2FeSiO4 is a kind of cathode material for lithium-ion electron. Because its crystal cell can allow two lithium atoms to be removed reversibly in theory, its theoretical specific capacity has a huge space to improve. At the same time, this material has the advantages of easy access to raw materials, pollution-free and low cost, and has been paid attention to by people. The doping of cathode material is considered to be an effective way to improve its electrical conductivity. By using the computer simulation technology based on the first principle method, this paper studies the effect of the structure and electrical conductivity of Cr doped Li2FeSiO4. The results show that the band gap of undoped Li2FeSiO4 is 2.44eV, and the band gap of Cr doped Li2FeSiO4 is reduced to 2.31eV, indicating that Cr doping can improve the electrical conductivity of Li2FeSiO4.

【關键词】硅酸铁锂;掺杂效应;计算机模拟

1 研究背景

锂离子电池主要由电极材料(正极和负极)、电解液和隔膜组成[1]。正极材料是锂离子电池的关键组成部分之一,其占锂离子电池约40%的成本,其优劣程度直接决定了锂离子电池的容量、电压、循环寿命等性能。其发展很大程度上影响了锂离子电池的发展。综合考虑性能与成本问题,正极材料主要筛选条件为原料廉价易得、制得电池安全无毒、制备工艺简单、有较高的放电电压(这就需要锂在体系中扩散系数高)、有较好的循环稳定性及循环使用寿命[2]。

聚阴离子型Li2FeSiO4是锂离子电池正极材料的研究热点之一,由于其晶胞理论上可允许可逆脱嵌两个锂,使得Li2FeSiO4理论比容量可达330mA·h/g,加上具有原料易得、无污染及成本低的优势,受到了人们的重视。计算机模拟研究表明Li2FeSiO4是半导体,导电性能较差,由于Li2FeSiO4电池中锂离子脱嵌数不超过1,所以Li2FeSiO4的实际实验容量只有166mA·h/g。……

登录APP查看全文