三维编织光固化3D打印复合材料的制备及力学性能
2018-09-10权利军李丹丹张春娥祝成炎
权利军 李丹丹 张春娥 祝成炎
摘要: 光敏树脂固化后的低强力一直是阻碍光固化3D打印技术发展的主要因素,利用三维编织织物的结构特点弥补光固化3D打印构件强力弱的缺点,文章重点研究了在光固化3D打印技术的基础上,结合三维编织技术制备3D打印复合材料的方式方法及对该种复合材料的力学性能进行测试分析。结果表明:三维编织光固化3D打印复合材料相对于纯光敏树脂材料,其弹性模量和拉伸断裂强度显著增加;高强聚乙烯纱线的增强效果最好,玻璃纤维纱线增强效果次之,碳纤维纱线增强效果最差。
关键词: 复合材料;光固化3D打印;三维编织;断裂强度;玻璃纤维;碳纤维
中图分类号: TS102.1;TB332文献标志码: A文章编号: 10017003(2018)02001306引用页码: 021103
Preparation and mechanical properties of photocuring 3D Printing composite
by threedimensional weaving
QUAN Lijun, LI Dandan, ZHANG Chune, ZHU Chengyan
(National Engineering Lab for Textile Fiber Materials and Processing Technology, Zhejiang SciTech University,
Hangzhou 310018, China)
Abstract: The low strength of the cured photosensitive resin has been a major obstacle to the development of photocuring 3D printing technology. The threedimensional braided fabric is used to make up the shortcomings of photocuring 3D printing component. This paper focuses on the study of photocuring 3D printing technology which was combined with threedimensional braiding technology to produce photocuring 3D printing composite material, and its basic mechanical properties. The results show that the elastic modulus and tensile fracture strength of photocuring 3D printing based on the threedimensional weaving are significantly higher than that of the pure photosensitive resin material. The reinforcing effect of the high strength polyethylene yarn is the best, followed by the glass fiber yarn, and the reinforcing effect of carbon fiber yarn is the worst.
Key words: composite materials; photocuring 3D printing; threedimensional weaving; breaking strength; glass fiber; carbon fiber
光固化3D打印技术是快速成型技术的一种,在近几年发展比较迅速,3D打印技术通常采用数字化的三维立体模型设计以逐层累积叠加的方式制作实物模型,是一种新型的快速成型制造技术[1],在现代工业中越来越受到重视。光固化3D打印技术的基本工作原理是通过特定波长的强光集束成一定形状的光影,再将光影投射入光敏树脂液中连續液态光敏树脂,形成一系列一定形状的固态树脂层片,然后在高度方向上累积叠加固化的树脂层片形成完整的三维立体实物模型[2]。材料的硬度、强度、塑性、延展性、弹性、脆性是表征复合材料的重要指标,然而固化后的光敏树脂一般强力较低,且尺寸精度较差,也正是由于固化后的光敏树脂强度较低且尺寸精度较差,光固化后的立体模型容易发生翘曲和形变[34]。……