摘 要:以菠萝叶纤维为原料,在氢氧化钠预处理后,通过酯化反应制备氯化血红素/菠萝叶纤维改性材料。采用氯化血红素对菠萝叶纤维进行改性,考察了氯化血红素质量浓度、接枝温度、反应时间对接枝率的影响,确定较佳接枝条件为氯化血红素质量浓度为1.0 g/L、反应时间2 h、接枝温度40 ℃。通过扫描电镜、红外光谱、X射线衍射及热重分析等,对菠萝叶纤维改性前后结构和性能进行表征。结果表明,改性纤维表面已接枝了氯化血红素,且半纤维素被去除;改性纤维仍属于Ⅰ型纤维素,结晶度由65.0 %提高到74.3 %,改性纤维的热稳定性降低。

关键词:菠萝叶纤维;氯化血红素;改性纤维

中图分类号:TS102.6

文献标志码:A

文章编号:1009-265X(2018)06-0023-06

Abstract:Pineapple leaf fiber was used as raw material to prepare materials modified with hemin/pineapple leaf fiber by esterification after sodium hydroxide pretreatment. Hemin was used to modify pineapple leaf fiber. The effects of hemin mass concentration, grafting temperature and grafting time on grafting rate were investigated. The optimal grafting conditions were confirmed as follows: mass concentration of hemin 1.0 g/L, grafting time 2 h, and grafting temperature 40 ℃. The structures and thermal properties of modified pineapple leaf fiber were characterized by scanning electron microscopy, Fourier transform infrared spectroscopy, X-ray diffractometer and thermogravimetric analysis. The results showed that hemin was grafted on the surface of the fiber and hemicellulose was removed. The crystal structure of modified fiber still belonged to cellulose Ⅰand the crystallinity increased from 65.0% to 74.3%. The thermal stability of the modified fiber decreased.

Key words:pineapple leaf fiber; hemin; modified fiber

菠蘿叶纤维又称菠萝麻,从菠萝叶片中提取得到,属于叶脉纤维。菠萝主要种植于中国广东、广西、海南、云南、福建和台湾省等地,年种植面积近60 000 hm2,每年产生的菠萝叶近1 000万t[1-3]。菠萝采摘以后,菠萝叶通常作为一种废弃物焚烧掉或者粉碎还田[4]。菠萝叶纤维具有透气、抑菌、除臭等性能,常被作为纺织材料生产纺织品,如袜子、内裤、毛巾、T恤、凉席等[5-7]。氯化血红素是一种具有羧基结构的天然金属卟啉化合物,主要存在于动物血液、肌肉细胞和植物组织中[8]。氯化血红素能在温和的条件下进行催化反应,它作为仿酶催化剂,具有很高的催化氧化活性。研究发现金属卟啉类物质可以催化氧化环境污染物并将其转化为无污染的物质[9-10]。……

登录APP查看全文