HFW焊管焊缝熔合线宽度的控制

胡松林

(宝钢股份有限公司钢管条钢事业部,上海201900)

为了合理地控制HFW焊管焊缝熔合线的宽度,提高焊管产品的焊接质量,以某规格3个钢级(B/X52/X60)高频焊管为例,按照API SPEC 5L及GB/T 9711的相关要求对焊缝性能进行了检测,分析了焊管母材化学成分对焊缝熔合线宽度及产品性能的影响。结果表明,HFW焊缝熔合线宽度随管线钢含C量下降而减小;对于焊接管线管,中部熔合线尺寸fn=0.02~0.08 mm,f0/fn=1.9~2.3,有利于预防加热不充分导致的不良焊接,也利于氧化物正常排出,从而保证HFW焊管产品的质量。

焊管;HFW;熔合线宽度

Abstract:In order to reasonably control the weld fusion line width of HFW pipe,increase the welding quality of welded pipe products,taking some specification three steel grade(B/X52/X60)HFW pipe as example,the weld properties were detected according to the relative requirements of API SPEC 5L and GB/T 9711.The results showed that HFW weld fusion line width reduce with pipeline steel carbon content reducing;for welded line pipe,the fusion line size(fn) of weld central section in the range of 0.02~0.08 mm,f0/fnis in the range of 1.9~2.3,It is helpful to prevent the harmful welding caused by the insufficient heating,and also helpful to the normal discharge of the oxide,so as to guarantee the quality of HFW welded pipe products.

Key words:welded pipe;HFW;fusion line width

1 HFW焊管的焊缝及其特征

1.1 HFW焊管的焊缝

HFW焊管是通过高频电流加热钢带对接边缘到熔融态,在不添加金属的情况下,通过挤压完成锻焊的制造过程。焊接过程中会在对接点熔融金属部位形成沙漏形熔池,部分金属得到氧化,在快速挤压时以氧化物形态排出,进而形成完整的焊缝。高温熔化的金属在焊接后的焊缝中心因氧化脱碳而颜色变浅,形成一条亮线,即熔合线。

对高频焊接后未进行热处理的焊缝部位取样、研磨和浸蚀后进行金相检测,结果如图1所示。由图1可以观察到完整的焊缝宏观形貌。

图1 高频焊管的焊缝形貌

通常情况下,将焊缝划分为熔合线(BL)、热影响区(HAZ)和母材区(B)3个部分。熔合线是指高频焊接后未进行热处理的焊缝中心区域,由于脱碳而出现的狭长亮线;热影响区是指焊缝区呈现出的一个双曲线形区域,在进行焊缝热处理后,随晶粒的均匀细化而消失;……