棉/粘胶弹力交织物的生物酶前处理工艺
2016-05-25岳仕芳
岳仕芳
(1. 常州纺织服装职业技术学院, 江苏 常州 213164; 2. 常州市新型纺织材料重点实验室, 江苏 常州 213164)
棉/粘胶弹力交织物的生物酶前处理工艺
岳仕芳1,2
(1. 常州纺织服装职业技术学院, 江苏 常州 213164; 2. 常州市新型纺织材料重点实验室, 江苏 常州 213164)
为减少织物损伤,降低前处理污水排放浓度和排放量,采用生物酶工艺处理棉/粘胶弹力交织物。采用渗透性和乳化性优异的表面活性剂与生物酶结合协同处理坯布,使坯布上的杂质发生生物降解、乳化、增溶,再结合氧漂工艺完成织物的前处理。采用平行试验与正交试验,考察织物的果胶去除率、毛细效应、白度、强力损伤率及排放污水的污染物浓度。结果表明:处理后织物果胶去除率达到89.3%;30 min毛细效应为9.5 cm;白度为85.9%;强力损伤率比常规生产的试样小;试样质量符合常规半制品的要求。该生物酶退煮与氧漂工艺产生废水的化学需氧量比常规工艺产生的废水低35.9%,废水的色度下降56倍,废水的pH值下降1.7,减排效果明显。
棉/粘胶弹力交织物; 前处理; 生物酶; 节能减排
Abstract In order to avoid fabric damage and reduce discharge concentration and quantity of waste water, a biological enzyme pretreatment process on cotton-rayon elastic fabrics was put forward. An efficient surfactant with excellent permeability and emulsifying properties was selected to combine with biological enzyme in the treatment of grey cloth. Therefore, the impurities on grey cloth were degraded, emulsified and solubilized. Then the oxygen bleaching process were conducted in the following pretreatment process. The removal rate of pectin, capillary effect, whiteness, strength damage rate and pollutant concentration were investigated by parallel and orthogonal experiments. The results showed that the removal rate of pectin reached 89.3%, capillary effect was 9.5 cm (30 min), and the whiteness reached 85.9%. The strength damage rate was less than that of conventional process. The sample quality meet the requirement of the semi-finished products. The COD value of wastewater was 35.9% lower than that produced during regular process. In the meanwhile, color degree reduced by 56 times and pH value decreased by 1.7 in comparison with the conventional process used in factory. The biological enzyme pretreatment process had obvious effect on emission reduction.
Keywords cotton/rayon elastic fabric; pretreatment; enzyme; energy conservation and emission reduction
棉/粘胶交织弹力直贡缎经向为全棉,纬向是粘胶氨纶包芯纱,吸湿排汗性好,穿着舒适,抗起皱性能改善,在市场上占有一定的份额[1]。粘胶纤维吸湿后显著膨胀,手感变硬,湿强力仅为干强力的1/2[2],经氢氧化钠(1.25 mol/L)处理8 min后强力损失达16%,用氢氧化钠(0.5 mol/L)处理相同时间后强力损失4.1%[3],耐酸、碱、氧化剂性能远低于棉纤维,因此印染前处理加工过程中应避免使用强碱浓碱[4]。棉/粘胶交织弹力坯布的杂质主要是棉经纱上的天然杂质和浆料,纬纱上的杂质主要是纺丝油剂。……